C400 Series Customized vacuum coating system

C400型多功能复合PVD离子镀膜设备是带有4套(靶直径160mm)多弧离子源蒸发源、2组多磁控溅射源、1组多功能蒸发源(选装)的实验涂覆薄膜的物理气相沉积真空镀膜设备。C400能同时安装多种不同的纯金属靶或合金靶材,在广泛应用的工业产品上镀制单层和多层薄膜。如应用于工具涂层和功能性涂层:切削工具、模具、冲具和各种关键的零组件(汽车、航空、航海、和其他设备上),以达到表面(在物理、化学、机械、光学、色泽等方面)改性的目的。

  • Sputtering, multi-arc composite coating process; complex coating series including DLC, amorphous, multi-layer film can be realized
  • Intelligent host computer control system for customized development of coating processes.
  • Nanny escort service, one-stop solution to coating center operation problems

The C400 is a customized unit that is stocked for the C-Series. HIPIMS and DLC functions are not included in the standard configuration. Nasi's self-use research and test coating machine is the C400 high-quality version, welcome to sample test.C400 PVD multi-functional coating machine price consists of: C400 customized coating machine; turn-key toolkit (Coating center plant construction package; equipment packaging, transportation, installation and commissioning, and training); customized coating process; according to the requirements of the optional.

Equipment Description

Main parameters and conditions of equipment operation

  • Occupied space: L4000×W2740×H2200mm
  • Coating effective area:φ680*H400
  • Power of the whole machine: actual work 50kw
  • Cooling water: pure water, PH value 6.5-8
  • Compressed air: rated pressure above 0.6Mpa
  • Process gases: Ar, H2, N2, C2H2, etc.
  • Equipment operating environment: temperature 15 ℃ -25 ℃, humidity ≤ 70%

Vacuum specifications (cold, empty, clean)

  • Ultimate vacuum: 8×10-4Pa
  • Pumping speed: ≤20 minutes
  • Pressure rise rate: ≤0.8Pa/hour
  • Heating temperature: 500℃
  • Electrical control system: PLC full automatic control
C400多功能复合真空镀膜机(images 1)

Mastery of core arc source technology - highly customizable

Adjustable magnetic field design ensures higher target utilization. Has a faster arc spot running speed, smaller arc spot, higher dissociation rate, smaller droplets, more conducive to the dissociation of low melting point targets.

Advantages of Laminators

  • Various cutting-edge technologies such as droplet-free high light arc, Hims, JVD high power, etc.
  • Deposition of multi-component, multi-structure, amorphous and other coating systems
  • Multiple coating technologies can be combined
  • High deposition rate, high film thickness uniformity, low coating defects

Dual-etching technology for dramatically improved bonding::

Based on more than 20 years of continuous operation and improvement, Naxau has developed a plasma etching technology SET and CET. Proper etching of the tool surface to achieve a clean and revitalized interface prior to coating is critical to a successful coating result. Etching requires the removal of surface contaminants such as metal oxides, water vapor, micro-oils and sweat debris. Etching also reactivates the surface and opens up molecular chains to induce ionic bonding during the coating process.

New Energy Coating

Wind Power Bearing Project

Wind Power Bearing Project Industry-University-Research Cooperation


In 2022, Naxau has successfully delivered the first PeCVD self-lubricating coating coater for wind turbine bearings, which significantly improves the life of wind turbines and reduces maintenance costs. Naxau, helping China's green power business to develop sustainably.

  • DLC load-bearing self-lubricating coating series
  • DLC, ta-C, Mo-containing super lubrication series, silicon doped coatings, etc.

Visit to the National Key Laboratory of High Performance Tools (Guangdong University of Technology)

Institutional Cooperation

Institutional Cooperation Transformation of Results


On October 31, 2023, Naxau undertook the transfer of two nano-hard coatings from the National Key Laboratory of High Performance Tools (Guangdong University of Technology) and signed a contract for the implementation of the transfer of the rights valued at RMB 1,200,000 yuan. In addition, Naxau also donated a set of multi-functional high-performance coating equipments valued at 5 million RMB to GDIT, which includes CET/SET side-to-side-through glow discharge etching system, CVC electrodeless magnetically-controlled arc source system, and UFC high light arc source system.