Site-wide search

Coating Solution for Cutting Tools

Knife Tool Coating SolutionsCutting tool coating solution

protective layerCoating DescriptionHardness
(HV)
film thickness
(μm)
antioxidant temperature
(°C)
coefficient of frictionAppearance ColorField of application
TNTiN20001.0~3.06000.25gold colorGeneral steel processing of taps
TiCNTiCN38001.0~3.04500.2grizzlyStainless steel and normal steel material processing of taps
TiAlNTiAlN30001.0~3.08000.4Purplish blackGeneral mold steel cutting processing
AMAlTi-based33001.5~3.09000.4grayish blackHRC≤40 mold steel, stainless steel cutting processing
ASMAlTiSi-based35001.5~3.010000.35grayish blackHRC≤45 mold steel, stainless steel cutting processing
HMTiSi-based38001.0~3.011000.3Bronze colorStainless steel, mold steel, titanium alloy cutting processing
HMATiSi-based42001.5~3.011000.3Bronze colorTitanium alloy, powder metallurgy steel, HRC30~55 mold steel processing
CVTiAlSi based35004~610000.3gold colorImitation CVD coating for turning inserts
APSAlCr-based35001.5~3.011000.3grayish blackHRC ≥ 40 mold steel cutting processing, stainless steel processing
AGAlCr-based35000.5~110000.3grayish blackStainless steel highlighting, high-gloss processing of special high-gloss
AMSTiAlCr-based36001.0~5.010000.3grayish blackHobbing, gear shaping cutters for various conditions, milling cutters, inserts HRC ≤ 50 mold steel, cast iron, etc.
AMTAlCr-based40001.0~3.010000.3grayish blackHigh-speed dry cutting of hobbing and gear shaping tools
AMLAlTi-based30001.0~5.010000.4BlackHRC≤45 mold steel, stainless steel cutting processing
AMRAlTiSi-based35001.0~5.011000.35Bronze colorFor hardened steel above HRC55
AUAlTiSi-based35001.0~5.011000.35Bronze colorSpecialized for PVD coating of stainless steel blades
DXCrAlTi-based32001.0~5.010000.4grizzlyGeneral purpose for milling and drilling up to HRC55
DAZrN-based30001.0~3.010000.3light golden yellowNon-ferrous metal processing, stainless steel processing, titanium alloy processing, high temperature alloy processing
AMDAlTiSi-based40001.0~3.012000.35grayish blackHigh-hardness mold steel machining, titanium alloy machining, high-temperature alloy machining
DHCrAlSi based35001.0~5.011000.35Bronze colorStainless steel milling, titanium cutting
DPAlCr-based32001.0~5.010000.3grayish blackHobbing tools for high-speed dry cutting, carbide tools for machining stainless steel, titanium alloy, mold steel
DTAlCrTiSi-based36000.5~311000.3Bronze color52-65HRC high hardness die steel, deharpenable alloys, wear-resistant materials, tungsten-copper alloys, composite materials
TX-SAlTi-based30001.0~5.06000.35gold colorCarbon steel blades up to HRC40 are universal
TiB2TiB230001.0~3.06000.3Greyish whiteNon-ferrous metal processing, plastics processing

High Gloss Arc Tool CoatingDroplet free coating

Droplet-free coating
CVD Blade Coating

Chemical Vapor Deposition Coatings

CVD coating


Naxau CVD Chemical Vacuum Vapor Deposition coating services are mainly focused on high hard cutting tools, anti-adhesive/stamping molding and other tooling categories.Naxau CVD can deposit coatings from 5 microns to 20 microns thick, using TiN, TiCN and α-alumina (Al2O3) to form monolayers or multilayers.The CVD deposition process is typically at 900°C or above, with a coating time of 10 hours, and is only for high temperature resistant substrates.

Razor Blade-ta-C Carbon Film

ta-C Coating for Thin Blade Cutters

Thin Blade Tool Coating


Naxau ta-C carbon film series, film thickness 0.2-0.5μm, hardness 3500-6000HV, coefficient of friction 0.1-0.15, low-temperature immersion film within 200℃, suitable for thin-blade knife tool applications. Skills significantly increase the cutting force without reducing the hardness and finish of the substrate, can be widely used in razor blades, lawn mowers, lint cutters, die cutters and other dry cutting conditions.

In addition, for thin-edged tools with high wear resistance requirements, NanoShield has a series of thick-film metal-ceramic films that can increase life by 2-4 times and reduce the risk of chipping.

刀具涂层方案(images 2)
刀具涂层方案(images 3)

TiB2 and ZrN for non-ferrous metals

Non-ferrous metal processing


NaxauTiB2 (titanium diboride) coating, 3000HV hardness, prepared by HiPiMS, low stress and high chipping resistance. Particularly suitable for non-ferrous metals (such as aluminum, copper, magnesium and its alloys) processing in the wear-resistant and anti-metal high-temperature corrosion working conditions. And it can realize 300 m/min high speed cutting; reduce 40% or more than traditional carbide.

ZrN chromium nitride coating, also widely used in non-ferrous metal processing and wood processing.

刀具涂层方案(images 4)
刀具涂层方案(images 5)