Array
Injection Screw - Injection Mold Coating
5068Surface hardness: 2000HV Coating thickness: 0.01-0.02mm Abrasion resistance: ★★★★ Corrosion resistance: ★★★★★ Anti-sticking ability: ★★★★ Applicable working conditions: high speed, high pressure, sticky material; for transparent optical products, all kinds of lenses, light guide plate, etc.; commonly used plastics for optical products: PMMA, PC, COC, COP, CR-39 and so on;reflect sth.
View Full Version