Nasi's high temperature resistant oxidizing-insulating PVD nano-coating
4899Gray-black, 600v insulation, 1-5 micron film thickness, 2800HV hardness, high temperature resistance over 700°, 0.3 low coefficient of friction. Multi-functional coatings, sampling and testing are welcome. ,