Forming Mold Coating Solutions
4434Coating Solution for Forming Molds Hardness: 30±1.5GPa Temperature MAX: 1100°C Working condition: oil-free lubrication Hardness: 2000HV or more Friction coefficient: 0.02-0.04 Maximum processing size: 1650mm Hardness: 2800-3500HV impact resistance (fatigue) good Hardness: 2000HV Aluminum adhesion resistance Good DLC Nash type CH. ZrN, CrO...