Site-wide search

View Categories

1.1-How to choose a PVD tool coating

summarize #

PVD nano-coating has become one of the three key elements of high-performance, high-precision tools. Precipitation hardening stainless steel, titanium alloys, high temperature alloys and other high-performance materials, the application of increasing, more difficult to process, the PVD coating process must continue to innovate to cope with the material has a higher hardness, tensile strength, adhesion, low thermal conductivity, hardened layer and other requirements at the same time, but also need to meet the environmental protection, high-speed cutting, dry cutting and other cutting processing of the new demands.

 


NanoShield PVD Blade Coating Guide #

Bronze Lathe Blade Coating

Depending on the specific shape of the insert, the machine parameters (process, speed, etc.), the material to be machined (heat treatment process, hardness, etc.), different PVD insert coatings are recommended.

For end customers, batch processing materials are fixed, you can choose stainless steel, high temperature alloys and other specialized blade coating. For distributors who need to prepare stock, they can consider general-purpose coatings to cope with the needs of different processing materials.

Coating NamecolorCoating hardness (HV)Antioxidant temperature ℃coefficient of frictionCoating thickness μmApplication Recommendations
Composite TiNgolden yellow20005000.252-3General-purpose steel processing; better adhesion resistance
TX-Sgolden yellow35008000.254-6General steel, cast iron, stainless steel universal coating
AMLPurplish black33008000.33-4General steel processing
AMRBronze color420010000.32-3For stainless steel, high hardness materials; wear-resistant and high temperature resistant
AMTgrizzly400012000.33-4For hard-to-machine materials such as high-hardness, nickel-based alloys, etc.

 


How to choose a hob coating #