Material Properties of TiB₂ (Titanium Diboride) Coatings #

TiB₂ (titanium diboride) is a quasi-metallic compound with a hexagonal crystal system structure, in which the boron atomic planes alternate with the titanium atomic planes in the crystal structure to form a unique two-dimensional mesh structure. The material has the following core properties:

  1. Ultra High Hardness: Mohs hardness of 9, after diamond (10), cubic boron nitride (9.8) and silicon carbide (9.5), room temperature microhardness of 2500~3300 kgf/mm², 600 ℃ still maintain the hardness level of Hv800;
  2. Excellent electrical conductivity: The resistivity is similar to that of metallic iron and platinum, and has a positive temperature coefficient characteristic and better conductivity than metallic titanium;
  3. chemical stability: Stable at room temperature in hydrochloric acid, dilute sulfuric acid, nitric acid and saturated oxalic acid, soluble only in hydrofluoric acid, slightly corrosive in concentrated sulfuric acid and dilute oxalic acid;
  4. High-temperature oxidation resistance: The block material has a maximum antioxidant temperature of 1100°C and maintains a hardness of 3.6 GPa and a flexural strength of 459 MPa at 1000°C.

Nasi TiB2 Coating #

  1. The TiB2 coating Y prepared using HiPiMS resulted in low coating stress Y improved the chipping resistance of the tool;
  2. The hardness of the coating is 39±2GPaY which gives the coating good resistance to abrasive grain wear;
  3. TiB2 coatings have low surface activity Y and titanium alloys ½ or easy chemical affinity ¾ less prone to adhesive wear, which in turn improves tool life;
  4. 4 Low surface roughness plating Y Increased chip removal performance Y Reduced friction Y Further improved tool life.
TiB2 special coating for non-ferrous metal processing
  • Hardness (HV)4000
  • Film thickness (μm)1
  • Oxidation resistance (°C)600
  • coefficient of friction0.3
  • Appearance Colorash gray
  • appliance Non-ferrous metal processing, plastics processing

TiB2 Coating Application Examples #