2.1-Does Nash provide free samples of PVD coating?

< 1 min read

Nasi provides free sampling service for regular PVD coatings, such as titanium nitride, titanium carbonitride, high alumina titanium, rose gold, silica-alumina-titanium, DLC and so on. However, it is only limited to small pieces that are processed with the furnace and do not need to be coated as a pendant.Proofing, risk of damage to artifacts!!!!

For daily opening of the furnace, the delivery time is 1-2 days. For regular opening of furnace, one week. (Delivery period may be extended due to power restrictions after October 2021)

R&D Collaborative R&D Programs #

After the research of Nasi, we believe that the customer's product has a great market prospect, and the customer's product is selected as the coating process for technical research, Nasi will sample free of charge until it succeeds or gives up. Welcome to call us for case studies.

 


 

Fee-based PVD Coating Proofing Service #

Nash actively promotes PVD functional coatings for new field applications and is willing to share R&D costs with test parties. We support the opening of experimental furnaces to provide non-conventional coatings / or customized vacuum coating processes. However, it is necessary to share the experimental data with the testing party.

  • Insulation Wear Resistant PVD Coating - Completed on September 31, 2021 and passed the customer's small test acceptance
  • High temperature anti-oxidation PVD coating--Completed on November 12, 2021, through customer pilot acceptance
  • Knife Belt Wear Coating - In Progress
  • High Viscosity Plastic Injection Mold Coating - In Progress

Difference between free PVD coating proofs and paid ones #

It is recommended that research institutes and customers with budgets use a dedicated furnace for long-term/repeatable follow-up of coating results.

 

Free SampleR&D Converter Proofing
Applicable Customerslow requirementsCoating results need to be tracked and repeatable
Vacuum equipmentfirefightingSpecialized furnaces; customizable coating parameters; guarantees optimal PVD coating results
Process Selectionnot haveType, film thickness (1-7 microns), arc source (sputtering/ion plating), uniformity, etching process, temperature/time, etc.
Coating typeConventional coatings such as TiNTheoretically, any coating that provides a target can be coated
delivery dateinconclusivefixed schedule
Coating QualityNaxi Factory StandardDelivery according to customer coating requirements
repetitivenot requiredSample blocks are available for inspection and can be guaranteed to be close to the quality of each batch.
dedicated engineernot haveDedicated Masters R&D Engineer / or team support
reverse engineeringnot haveSimilar coatings can be copied from customer samples
Certificate of qualification machineNaxos available/ or not availableAssistance with third-party national professional certificates is available