Site-wide search

Coating Solution for Forming Molds

Naxau Molding Die Coating Solutionsour products and services

DLC Naxau model CH. For new mold coatings such as ZrN, CrO, etc., please download the latest Naxau coating catalog.

protective layerCoating DescriptionHardness
(HV)
film thickness
(μm)
antioxidant temperature
(°C)
coefficient of frictionAppearance ColorField of application
TRNCrN20004~107000.4ash grayTitanium alloy hot forging, aluminum sheet stamping
ARSCrAlTi-based36004~710000.6grayish blackHigh-strength plate stamping
AMCCrAlTi-based38004~74000.2rose gold colorStainless steel mold stamping
ARPCrAlTiN-based36003~511000.5grayish blackStainless steel hot stamping, fine blanking, bar punching, etc.
ARKCrN-based18003~56000.6ash grayPlastic molds, semiconductor packaging molds general purpose coatings
ARDCrO-based28003~612000.6dark coloredHigh-temperature wear-resistant parts, high-temperature electrical insulation parts, corrosion-resistant and wear-resistant parts
DECrAl-based30004~710000.5grayish black≤ 500MPa general steel plate stamping, non-ferrous metal processing mold class, die casting molds
DECCrAlTi-based38004~74000.2rose gold colorStainless steel mold stamping, high strength plate, deep drawing type processing molds
CHa-C:H20001-33000.1-0.2BlackGeneral purpose solid lubricant coatings for self-lubricating parts and non-ferrous metal machining

F-DLC Tire Mold Coating

F-DLC Coating


Hydrophobicity is a prerequisite for tire molds to achieve easy release, anti-sticking and self-cleaning functions.

Coating for Integrated die-casting mold

Integrated Die Casting Mold Coating


The Dura process improves the bonding between the coating and the substrate and is a viable alternative to TD or CVD coatings. Low temperature coating process, no deformation of the substrate and consistent hardness. Compared with TD, it has higher surface hardness, pressure resistance and high temperature resistance. For die casting mold inserts, it can be up to 5 times or more fading titanium re-plating.

PVD Coating for Mirror Molds

PVD Mirror Mold Coating


Naxau has a wide range of mirror/ultra-mirror mold coating series with good anti-polymer sticking function. Such as TiN coating for electron gun process, which is commonly used in plastic molds; CrN for magnetron sputtering process, which is commonly used in coated mold heads; and ta-C amorphous high temperature resistant super hard carbon film from Hipims, which is commonly used in high borate blister glass molds.

Cylinder mold processing

PVD Coating for Forming mold

Forming Mold Coating Solutions


Over the past 22 years, Naxau has experience in coating applications for a wide range of industries, including injection molds, stamping dies, forging dies, extrusion/stretching dies, and glue wood molds.