With provincial R&D labs and factory QC labs, Naxi has perfect coating characterization test instruments to provide reliable customized and standardized PVD nano-coatings for customers. We can provide nano-coating composition analysis, bonding force, film thickness, surface hardness, friction, roughness, impact resistance, insulation, high temperature resistance and other test checks.

Naxau PVD nano-coating R&D technology platform

Naxau PVD Coating Technology Platform

Nash Coating Analytical Laboratory

7th generation high light arc SPARK droplet-free PVD nano-coating

7th Generation Spark Droplet-Free PVD Coatings

NanoShield Droplet-Free Coating

PVD coating surface, under 10,000 times the electron microscope can be observed in the naked eye can not see the details, which multi-arc ion plating and magnetron sputtering have many droplets.

To get nanomaterials right, you have to work on what you can't see with the naked eye. The cornerstone of a nano-coating is the molecular clusters in each plasma, and if the plasma is defective, the nano-coating that grows out of it will be faulty. NanoShield's scientists have persisted for years in developing the most technically challenging SPARK high light arc droplet-free nano-coating in the hope that perfect nanocrystals will grow out of the defect-free plasma to deposit the best possible nano-coating. This dream has been realized with the droplet-free platform of NanoShield SPARK 7. SPARK 7 ensures the stability of PVD-coated products over long periods of time, knowing that a single 1-micron coating droplet destroys a machined product with 5-micron precision requirements. A single defect on a tool's edge can cause cutting lines on the part being machined. Just one droplet on a mold also causes a spot on the machined product as well, neither of which are acceptable results for modern machining.

Dubba Composite PVD Coating Technology

DURA Composite PVD Coating Technology

Dubba Composite Coating Technology

Naxau PVD Coating Wizard (Partial)

Selected Naxau PVD Coatings

Coatings for cutting tools

protective layerCoating DescriptionHardness
(HV)
film thickness
(μm)
antioxidant temperature
(°C)
coefficient of frictionAppearance ColorField of application
TNTiN20001.0~3.06000.25gold colorGeneral steel processing of taps
TiCNTiCN38001.0~3.04500.2grizzlyStainless steel and normal steel material processing of taps
TiAlNTiAlN30001.0~3.08000.4Purplish blackGeneral mold steel cutting processing
AMAlTi-based33001.5~3.09000.4grayish blackHRC≤40 mold steel, stainless steel cutting processing
ASMAlTiSi-based35001.5~3.010000.35grayish blackHRC≤45 mold steel, stainless steel cutting processing
HMTiSi-based38001.0~3.011000.3Bronze colorStainless steel, mold steel, titanium alloy cutting processing
HMATiSi-based42001.5~3.011000.3Bronze colorTitanium alloy, powder metallurgy steel, HRC30~55 mold steel processing
CVTiAlSi based35004~610000.3gold colorImitation CVD coating for turning inserts
APSAlCr-based35001.5~3.011000.3grayish blackHRC ≥ 40 mold steel cutting processing, stainless steel processing
AGAlCr-based35000.5~110000.3grayish blackStainless steel highlighting, high-gloss processing of special high-gloss
AMSTiAlCr-based36001.0~5.010000.3grayish blackHobbing, gear shaping cutters for various conditions, milling cutters, inserts HRC ≤ 50 mold steel, cast iron, etc.
AMTAlCr-based40001.0~3.010000.3grayish blackHigh-speed dry cutting of hobbing and gear shaping tools
AMLAlTi-based30001.0~5.010000.4BlackHRC≤45 mold steel, stainless steel cutting processing
AMRAlTiSi-based35001.0~5.011000.35Bronze colorFor hardened steel above HRC55
AUAlTiSi-based35001.0~5.011000.35Bronze colorSpecialized for PVD coating of stainless steel blades
DXCrAlTi-based32001.0~5.010000.4grizzlyGeneral purpose for milling and drilling up to HRC55
DAZrN-based30001.0~3.010000.3light golden yellowNon-ferrous metal processing, stainless steel processing, titanium alloy processing, high temperature alloy processing
AMDAlTiSi-based40001.0~3.012000.35grayish blackHigh-hardness mold steel machining, titanium alloy machining, high-temperature alloy machining
DHCrAlSi based35001.0~5.011000.35Bronze colorStainless steel milling, titanium cutting
DPAlCr-based32001.0~5.010000.3grayish blackHobbing tools for high-speed dry cutting, carbide tools for machining stainless steel, titanium alloy, mold steel
DTAlCrTiSi-based36000.5~311000.3Bronze color52-65HRC high hardness die steel, deharpenable alloys, wear-resistant materials, tungsten-copper alloys, composite materials
TX-SAlTi-based30001.0~5.06000.35gold colorCarbon steel blades up to HRC40 are universal
TiB2TiB230001.0~3.06000.3Greyish whiteNon-ferrous metal processing, plastics processing

Carbon Film Coating

protective layerCoating DescriptionHardness
(HV)
film thickness
(μm)
antioxidant temperature
(°C)
coefficient of frictionAppearance ColorField of application
C Ha-C:H1500-25001~53000.1~0.2BlackGasoline engine valve train and piston, pump, compressor, bearing outer ring, etc.
C HSa-C:H:Si1500-25001~54000.1~0.2BlackPlastic injection-molded sliding parts, aluminum sheet stamping dies, medical parts, etc.
C RHCrN+a-C:H1500-25002~53500.1~0.2BlackDiesel engine parts, soft base materials (e.g. aluminum or copper), pumps, compressors, etc.
C HWWC/C1000-15001~43000.1~0.2grayish blackGears and ball bearings, highly precise internal combustion engine components, etc.
C TAta-C50000.2~25000.1~0.2Brilliant color or grey-blackDrilling, milling, countersinking, reaming tools for machining non-ferrous metals, synthetic materials, organic materials, etc.
C Aa-C30001~54000.1~0.2grayish blackAluminum sheet trimming, plastic injection molding, ejector pins, guide pins and bushings, mold sliding parts, etc.
Diadiamonds100001.0~126000.02~0.1dark grayGraphite, Composites, Carbon Fiber

Mold Coating

protective layerCoating DescriptionHardness
(HV)
film thickness
(μm)
antioxidant temperature
(°C)
coefficient of frictionAppearance ColorField of application
TRNCrN20004~107000.4ash grayTitanium alloy hot forging, aluminum sheet stamping
ARSCrAlTi-based36004~710000.6grayish blackHigh-strength plate stamping
AMCCrAlTi-based38004~74000.2rose gold colorStainless steel mold stamping
ARPCrAlTiN-based36003~511000.5grayish blackStainless steel hot stamping, fine blanking, bar punching, etc.
ARKCrN-based18003~56000.6ash grayPlastic molds, semiconductor packaging molds general purpose coatings
ARDCrO-based28003~612000.6dark coloredHigh-temperature wear-resistant parts, high-temperature electrical insulation parts, corrosion-resistant and wear-resistant parts
DECrAl-based30004~710000.5grayish black≤ 500MPa general steel plate stamping, non-ferrous metal processing mold class, die casting molds
DECCrAlTi-based38004~74000.2rose gold colorStainless steel mold stamping, high strength plate, deep drawing type processing molds